1708 fiberglass cloth is a stitched, ±45° biaxial reinforcement with a chopped strand mat layer on one face. Builders choose it where a part twists or shears and where laminate thickness has to build quickly: boat hulls and stringers, wind blade skins, chemical tanks and sports gear. Despite the name, it is not a woven cloth, and that detail drives most buying decisions.
This guide gives the specification table first, then the features with the evidence behind them, then where it is used and why, and ends with a buying checklist. Performance figures are separated into what is established and what you should verify on your own laminate.
What 1708 Fiberglass Cloth Actually Is

The 1708 code describes a two-layer build. The first layer is 17 oz per square yard of ±45° biaxial fabric. Stitched to it is a chopped strand mat layer of 0.75 oz per square foot, which is the “08” in the code.
The same construction is sold as 1708 composite cloth, biaxial mat and ±45° combo mat. A plain biaxial fiberglass cloth is the ±45° fabric without the mat layer. Do not buy by name. Treat 1708 fiberglass cloth as a construction to specify: biaxial weight, mat weight, glass type, stitching and width. If two quotes carry the same name but differ on any of those, they are different products.
Specification Table
The table below puts 1708 fiberglass cloth and its two mat variants side by side. Metric figures are conversions from the listed ounce values, so confirm them against the datasheet.
| Parameter | 1705 | 1708 (Standard) | 1715 |
| Biaxial layer | ±45°, 17 oz/yd² (about 576 g/m²) | ±45°, 17 oz/yd² (about 576 g/m²) | ±45°, 17 oz/yd² (about 576 g/m²) |
| Mat layer | 0.5 oz/ft² (about 153 g/m²) | 0.75 oz/ft² (about 229 g/m²) | 1.5 oz/ft² (about 458 g/m²) |
| Approx. total weight (calculated, excludes stitch thread) | about 730 g/m² | about 805 g/m² | about 1,035 g/m² |
| Intended use | Thinner profiles | General laminating | Impact-prone panels, larger resin zone between plies |
| Glass options | E-glass, ECR, fine-surface | E-glass, ECR, fine-surface | E-glass, ECR, fine-surface |
| Resin systems | Epoxy, polyester, vinyl ester | Epoxy, polyester, vinyl ester | Epoxy, polyester, vinyl ester |
| Layer joining | Stitching | Stitching | Stitching |
One unit issue needs attention. The 1708 page gives the mat as 0.75 oz per square foot but adds a bracketed “approx. 8/10 oz”, which does not match that unit. The conversion of 0.75 oz/ft² is about 229 g/m², in line with the 225 g/m² chopped strand mat grade. Ask for the datasheet in g/m² to avoid mistakes.
Key Features and Why They Matter

±45° fiber direction. Fibers sit at an angle to the length of the part, so in-plane shear and twist load them along their length. That is the engineering reason ±45° plies are used in hull skins and blade shells. A 0°/90° weave is aligned to axial loads instead. This does not make a laminate stronger in every direction. Real laminates usually combine ±45° and 0° layers.
Non-crimp structure. In a woven fiberglass fabric, yarns bend over and under each other. Laboratory work on non-crimp fabric laminates found that more tow crimp lowered compression strength, and that crimp and resin-rich areas depended on tow spacing, stacking sequence, stitch density and stitching material. Straighter fibers are a real advantage in compression-loaded parts, but stitching is not neutral. Poor stitching can bring its own defects, so check the stitch details and not only the words “non-crimp”.
Stitched reinforcement, not an adhesive layer. The plies are held by thread. The argument is simple: fewer chemicals between plies and open channels for resin. Testing evidence is mixed on interlaminar benefits. A study of stitched multiaxial warp-knit composites found that stitching parameters had little effect on flexural and interlaminar shear properties, apart from stitch location. Do not expect stitching alone to raise shear performance. Resin choice, fiber content and void control matter more. If you use epoxy, ask whether the mat layer carries any binder, because binder compatibility with epoxy is the reason stitched mats exist.
Mat layer. It builds thickness quickly and gives resin a flow path between plies. Ask your laminate designer how much structural credit, if any, to give it. Many designers treat it mainly as bulk and a flow layer.
Resin use. Savings against woven roving are plausible but depend on your process and reference laminate. See the next section.
For deeper reading, the book Non-Crimp Fabric Composites: Manufacturing, Properties and Applications has separate chapters on stitching effects, damage progression, fatigue and wind turbine use.
Performance Claims: What Is Established and What To Test
Product data for 1708 fiberglass cloth includes several performance figures. None come with a published test method, so treat them as targets to confirm.
| Claim | Source and Basis | What It Can Tell You | How To Verify |
| Up to 30% less resin than woven roving | 1708 product page. Test method, resin, process and comparison laminate are not published | The direction of a saving, not a number to budget on | Build one panel with 1708 and one with your current reinforcement at equal thickness. Weigh each dry stack and cured panel, then compare resin by weight. Fiber content can be checked per ASTM D3171 |
| Up to 15% less waste | 1708 product page. Baseline not published | A saving exists only where custom widths replace trimmed standard widths | Draw a cut plan on your molds for standard and custom widths. Waste % = (area bought – area used) / area bought |
| Less micro-cracking | Product page. No data published | Removing fiber waviness removes one stress concentrator. Cracking also depends on resin toughness, fiber content, cure and laminate design | Ask for test data. For fatigue-critical parts, run your own cyclic test |
| Better interlaminar shear | Product page. No values published | Binder-free joining may help with epoxy. Shear strength also depends on resin-rich layers and voids | Short-beam shear on matched panels (ASTM D2344 or ISO 14130), same resin and process |
| Impact resistance | Product page. No data published | A thicker mat layer is a design option, not a proven result | Drop-weight impact test (ASTM D7136) on your laminate |
| Faster wet-out | Product page | Plausible, since the mat layer gives resin a path. Depends on resin viscosity, process and stitch pattern | Time full saturation on your own resin and process |
| Longer fatigue life than 0°/90° weaves | Product page. Basis not published | An orientation advantage for shear-dominated loads, not a guarantee of laminate fatigue life | Review with your designer, and see the NREL point under wind blades below |
One more reason to test the resin figure. In the Cranfield study, thicker resin layers lowered interlaminar shear strength. A laminate that saves resin through compact fiber packing can be better on both counts, but a laminate with resin-rich lines from stitching or poor wet-out can be worse. Weight alone will not tell you which one you have.
The Three Grades
Grade | Best For | Why |
| Standard E-Glass | Boat hulls, automotive panels, sports equipment | Balanced mechanical toughness at the most competitive price point |
| ECR-Glass | Chemical tanks, scrubbers, offshore marine infrastructure | Boron-free structure resists acid leaching and alkaline attack |
| Fine-Surface | Master molds, high-gloss aesthetic parts | Ultra-thin tissue on the face prevents print-through of fiber texture |
Where It Is Used and Why

Boats and Marine Composites
It is used in hulls, transoms and internal stringers. Why: a hull flexes against waves, and slamming and torsion load panels in shear, not only in bending. ±45° fibers sit in line with that shear. The mat face builds thickness quickly where heavy sections are laminated by hand. Stringers are often wrapped with slit tapes, and locked-edge stitching on narrow widths keeps them from fraying on vertical or overhead lay-ups. For marine composites, standard E-glass covers most hulls, while ECR suits offshore infrastructure with acid or alkaline exposure. The fiberglass mat for boats range covers the related mat products.
Check: resin compatibility, slit widths for tapes, and the mat weight with your designer. 1715 is meant for impact-prone panels, but confirm that with a drop-weight test, not the name.
Wind Blades

It is listed for blade spars and roots. Why: a blade shell acts as a torsion box, and ±45° glass carries the shear. Public research supports the use, with a caveat. A US Department of Energy blade study lists a 1708-style ±45° fabric with mat among the fabrics in a 9 m test blade, noting that double-bias fabrics cover most of the skin area. NREL fatigue testing of laminates combining 0° and ±45° layers found fatigue resistance varied with fiber content and the share of ±45° reinforcement, and was poorer than expected at high fiber contents and high ±45° proportions.
The lesson is that this fiberglass reinforcement carries shear, not everything. Where bending along the length dominates, the laminate needs 0° layers as well.
Check: the ±45° share and fiber content with the blade designer, and batch weight and width results so the schedule holds from roll to roll.
Automotive and Transport
Racing bodies, chassis reinforcement and truck panels. Why: resin-to-weight ratio matters, and a fabric that lies down on a curved tool avoids wrinkles and resin-rich pockets. ±45° plies also suit panels that see twisting loads.
Check: drape on the tightest radius of your actual tool, not on a flat bench. If the mat layer adds more thickness than the part allows, specify 1705.
Industrial Corrosion Containment

Chemical storage tanks, flue gas desulfurization units and scrubbers. Why: standard E-glass can be embrittled by acid leaching and alkaline attack, so the ECR grade uses a boron-free structure. The mat layer builds wall thickness steadily, and ±45° plies add shear support.
Check: the resin must resist the same chemicals, because glass is only half of the barrier. Give your resin supplier the chemical list, concentrations and temperatures, and get ECR named on the datasheet. Standard E-glass is not the right choice for chemical service.
Sporting Goods
Surfboard stringers, sculling boats and skis. Why: these parts are flexed and twisted repeatedly, so shear-aligned fibers and a thin laminate matter. For slim profiles, 1705 keeps the mat layer light. For gloss surfaces, the fine-surface grade reduces fiber print-through.
Check: weigh a finished test part against your target, and inspect a fine-surface sample under raking light before volume.
How To Choose the Right Specification For Your Project
When you specify 1708 fiberglass cloth, settle these in order.
- Dominant load. Twist and shear point to 1708. Bending along one axis needs added 0° reinforcement.
- Glass. Standard E-glass for general work, ECR for acid or alkaline exposure, fine-surface for show faces.
- Mat weight. 1705 for thin profiles, 1708 as the default, 1715 for impact-prone panels.
- Resin and process. Confirm your resin system and whether you use hand lay-up or vacuum infusion.
- Widths. Match slit widths to your molds and cut plan.
- Layer count. Confirm with your laminate designer, not by guesswork.
| Project | Grade | Mat | Reason |
| Hull or transom | Standard E-glass | 1708 | Shear and twist loads, quick thickness build |
| Stringer wrapping | Standard E-glass, slit rolls | 1708 | Locked-edge tapes stay intact |
| Impact-prone panels | Standard E-glass | 1715 | Thicker mat zone, confirm by test |
| Thin sports profiles | Standard E-glass | 1705 | Lower laminate thickness |
| Tanks and scrubbers | ECR | 1708 | Acid and alkaline resistance |
| Master molds, show faces | Fine-surface | 1708 | Reduces fiber print-through |
Buying Guide: What To Confirm Before You Order
Specifications To Confirm
| Parameter | Published | Ask For | Why It Matters |
| Biaxial weight | 17 oz/yd² | Datasheet in g/m² with tolerance, test method (ASTM D3776) | Sets laminate weight and resin demand |
| Mat weight | 0.5, 0.75 or 1.5 oz/ft² | Units and tolerance in writing | Thickness build and resin flow |
| Total weight | Not published | Confirmation of the calculated figure | Needed for your laminate schedule |
| Thickness | Not published | Dry thickness (ASTM D1777) and cured thickness per ply from a test panel | Decides layer count |
| Glass grade | E, ECR, fine-surface | Grade named on datasheet and quote | Chemical service and surface finish |
| Fiber angle | ±45° | Whether other angles are available | Matches the load direction |
| Stitch details | Stitched | Stitch type, gauge, thread material | Affects wet-out, print-through and resin-rich lines |
| Mat-layer binder | Not published | Whether any binder is present, and which | Epoxy compatibility |
| Width | Slit 4 to 100 inches | Standard roll width and custom options | Cut plan and waste |
| Roll length, core, roll weight | Not published | Length, core diameter, kg per roll, packing | Handling and shipping |
| Tolerances | Not published | Weight and width tolerances as numbers | Repeatability between rolls |
Customization Options
| Option | Range | Use It When |
| Mat weight | 1705, 1708, 1715 | You need to tune thickness or impact performance |
| Glass grade | E-glass, ECR, fine-surface | Chemical exposure or a show face |
| Slit width | 4 to 100 inches, locked edges | Stringer tapes and mold-matched widths |
| Length and labeling | Customizable across the fabric range, confirm for 1708 | Your logistics or inventory system needs it |
Compare Quotes on the Same Basis
Two quotes both saying “1708” are comparable only if biaxial weight, mat weight, glass type, stitching and width match. Put those five side by side first. Then compare cost per finished panel, not per roll, using your own resin and waste measurements from the claims table.
Approve a Sample With Numbers
| Check | Method | A Good Result |
| Layer weights | Weigh a cut sample | Within the agreed tolerance |
| Width and edges | Measure, cut and handle | Within tolerance, no unraveling |
| Wet-out | Time saturation with your resin | Consistent, no dry spots |
| Resin use | Weigh dry stack and cured panel | Matches your target |
| Cured thickness per ply | Measure the panel | Fits your layer count |
| Shear or impact, if the part needs it | ASTM D2344 or D7136 | Meets your design value |
Verify the Supplier
A good sample proves one roll, not the next delivery. ZS Fiberglass lists incoming material inspection, in-line inspection, final inspection and customer AQL checks, with in-house lab testing for pull strength and for weight and thickness. Ask for batch results on your own order and how repeat orders are held to the same construction. Commercial terms listed are a 15-day lead time for fiberglass raw materials, a 1-year warranty, free A4 samples, and a 30% deposit with 70% before loading for new customers. Ask how long locked-in pricing runs.
FAQs
1.Is 1708 Fiberglass Cloth a Woven Fabric?
No. It is a stitched, non-crimp construction: a ±45° biaxial layer joined to a chopped strand mat. Calling it cloth is common, but you should specify it by construction.
2.What Does 1708 Mean?
It refers to 17 oz per square yard of biaxial fabric plus a mat layer, listed as 0.75 oz per square foot. Confirm the exact weights on the datasheet, because suppliers describe the mat in different units.
3.Which Grade Should I Choose?
Standard E-glass for hulls, panels and sports gear, ECR for acid or alkaline exposure, and fine-surface where print-through matters on a high-gloss face.
4.When Should I Choose 1705 or 1715 Instead?
Choose 1705 for thinner profiles and 1715 where high-impact resistance and a larger interlaminar zone matter. Standard 1708 suits most general work.
5.How Should I Approve a Sample?
Check weight, width and stitching against the datasheet, then laminate a test panel with your resin and process. Look at wet-out, air voids, drape and edge stability.